Bitumen PenetrationPenetration Grade ASTM

Bitumen 200/300 Dubai UAE

Share this article

Bitumen 200/300

Bitumen 200/300

Bitumen Penetration Grade 200/300

Bitumen penetration grade 200/300 bitumen means the penetration value is in the range of 40 to 50 at standard test conditions which are commonly used as a Paving Grade. Also, Bitumen is applicable for the production of hot mix asphalt for bases and pavements and for road construction.

asphalt is specified by the penetration and softening point test. Designing is by penetration range only.

the penetration grade asphalt has a thermoplastic property which causes the material to soften at high temperatures and to harden at lower temperatures.

Properties of Bitumen 200/300

Bitumen Penetration Grade 200/300 is categorized based on its penetration and viscosity attributes, which indicate its consistency and workability. The numeric values denote the penetration depth in tenths of a millimeter at a standard temperature of 25°C. Let’s delve into the key properties that make Bitumen 200/300 a cornerstone of construction:

  1. Penetration Depth: Falling within the penetration range of 200 to 300, Bitumen 200/300 possesses a harder consistency. This characteristic imparts strength and stability to structures, making it suitable for a variety of applications where durability is paramount.
  2. Viscosity: Bitumen 200/300 exhibits moderate viscosity, allowing for efficient mixing with aggregates. This property facilitates the creation of uniform and durable asphalt mixes that can withstand the challenges posed by heavy traffic and diverse climatic conditions.
  3. Adhesion: With excellent adhesion properties, Bitumen 200/300 ensures a strong bond between bitumen and aggregates. This quality plays a pivotal role in the formation of robust road surfaces that resist aggregate displacement and enhance overall road stability.
  4. Durability: The inherent elasticity of Bitumen 200/300 enables it to accommodate temperature-induced expansion and contraction, contributing to the durability and long-term performance of roads and structures.

Application of Bitumen 200/300

Bitumen Penetration Grade 200/300 finds widespread utilization across a spectrum of construction domains, playing a vital role in infrastructure development:

  1. Road Construction: A primary application of Bitumen 200/300 lies in road construction, where it serves as a critical binder in asphalt mixes. Its robust properties contribute to the creation of resilient road surfaces that can endure heavy traffic loads and environmental challenges.
  2. Pavement Preservation: In pavement preservation treatments, such as chip seals and slurry seals, Bitumen 200/300 offers a reliable solution to extend the lifespan of existing roads. It prevents crack formation, shields against water penetration, and enhances skid resistance.
  3. Industrial Applications: Beyond road construction, Bitumen 200/300 finds utility in the industrial sector, where it is employed in the formulation of coatings, adhesives, and sealants, catering to a wide range of applications.

Guaranty and safety of Bitumen Penetration Grade 200/300

BituKim guaranty the quality of bitumen penetration grade 200/300 with the arrangement of the international inspectors to check the quality and quantity of the bitumen penetration grade 200/300 during the loading to the vessel and controlling the production by QC by batch test report before shipping. BituKim Company guarantees the quality to meet with ASTM.

Packing Of Bitumen Penetration Grade 200/300

  •  180kg New Steel Drum: Loading 110 Drum in 20 ft
  • 375Kg Bitubag: Loading 24 MT in 20 ft Container
  • Bulk in vessel: Loading 2000 to 20,000 MT in Bitumen Carrier
  • Bulk in Flexi Bag: Loading 20 MT in Bitumen Felexi Bag
  • Bulk in Tunker: Loading 25 MT in Truk Tanker

Specification of bitumen penetration grade 200/300

BITUMEN 200/300TEST METHOD UNITSPECIFICATION
Specific gravity @ 25/25 °cASTM D70Kg/cm³990-1040
Penetration @ 25°cASTM D5mm/10200-300
Softening point °cASTM D36°C32
Ductility @ 25°cASTM D113cm100 min
Loss on heating(wt) %ASTM D6wt %1 max
Drop in Penetration after heating %ASTM D5-D6%37 max
Flashpoint °cASTM D92°C177 min
Solubility is CS2(wt) %ASTM D4wt %99 max
Spot testA.a.s.h.o.t102-Negative

Leave a Reply

Your email address will not be published. Required fields are marked *

Fill out this field
Fill out this field
Please enter a valid email address.
You need to agree with the terms to proceed

Menu